Grey cast iron holds carbon in the form of____________________?
Show answer Hide answer
Answer: C. flakes
Explanation
Grey cast iron contains carbon exceeding the solubility limit of austenite during solidification cooling. This excess carbon precipitates out of the iron matrix in the structural form of graphite flakes. The exposed graphite flakes dictate the mechanical properties and machinability of grey iron components. Cast irons are iron-carbon alloys containing more than two percent carbon along with silicon additions. Graphite flakes act as internal stress concentrators, giving grey iron excellent vibration damping capabilities. The fractured surface appears grey because light reflects off the exposed crystalline graphite flake structures.
Automotive engine cylinder blocks and machine tool frames are manufactured from grey cast iron for rigidity. The excellent damping capacity of grey iron absorbs mechanical vibrations in heavy industrial machinery bases. Brake rotors utilize grey cast iron due to its thermal conductivity and resistance to thermal distortion. Cementite represents iron carbide, which is characteristic of white cast iron rather than grey cast iron. Nodular and spheroidal graphite structures occur in ductile cast iron rather than standard flaky grey iron. Free carbon in flake form specifically defines grey iron, separating it from alloyed or malleable iron types.
- Subject
- Engineering
- Category
- Mechanical Engineering
- Topic
- —
- Difficulty
- medium
Related questions
Q1. Within a static fluid___________________?
Show answer Hide answer
Answer: D. only normal stresses can exist
In a static fluid at rest, shear stresses cannot exist by definition. Fluid molecules at rest do not slide past one another, eliminating any internal resistance to shear. Therefore, only normal compressive stresses, comm...
Q2. Nodular iron contains graphite structured as_____________________?
Show answer Hide answer
Answer: D. spheroids
Nodular cast iron contains graphite arranged in distinct spheroidal or nodular shapes. Special treatment of the molten metal transforms sharp graphite flakes into rounded spheres. Spheroidal graphite stops stress concent...
Q3. Malleable iron contains carbon presented as___________________?
Show answer Hide answer
Answer: E. nodular aggregates of graphite
Malleable cast iron is produced by heat treating white cast iron through a prolonged annealing process. This thermal treatment causes cementite to decompose into stable irregular nodular aggregates of graphite. These gra...
Q4. Advancing spark timing in petrol engines results in_______________?
Show answer Hide answer
Answer: A. increase the knocking tendency
Advancing the spark timing causes combustion to occur earlier while the piston is still rising. This premature burning creates extreme peak pressures inside the cylinder chamber. Higher peak pressures dramatically increa...
Q5. Locomotive boilers restrict maximum steam pressure to_______________?
Show answer Hide answer
Answer: D. 18 kg/cm2
Traditional locomotive boilers are restricted to moderate operating pressures around eighteen kilograms per square centimeter. Structural limitations of fire tube designs prevent safely containing higher steam pressures....
Q6. Supercharging a petrol engine operating on fixed-octane fuel and constant compression ratio will_________________?
Show answer Hide answer
Answer: A. increase the knocking tendency
Supercharging increases the density and pressure of the air-fuel charge entering the engine cylinder. Higher charge density leads to increased peak combustion temperatures and pressures during the power stroke. These ele...