Malleable iron contains carbon presented as___________________?
Show answer Hide answer
Answer: E. nodular aggregates of graphite
Explanation
Malleable cast iron is produced by heat treating white cast iron through a prolonged annealing process. This thermal treatment causes cementite to decompose into stable irregular nodular aggregates of graphite. These graphite nodules relieve internal stress and provide the material with superior ductility and toughness. White cast iron is extremely hard and brittle because its carbon is combined chemically as iron carbide cementite. Annealing white cast iron transforms the microstructure into a ferrite or pearlite matrix containing temper carbon nodules. Malleable iron combines the ease of casting with mechanical properties that approach low carbon steel grades.
Option A is incorrect because cementite is the hard brittle carbide found in untreated white cast iron. Option C is wrong because graphite flakes are characteristic of grey cast iron rather than malleable iron. Options D and E require precision, but option E correctly identifies the specific nodular form of graphite aggregates.
- Subject
- Engineering
- Category
- Mechanical Engineering
- Topic
- —
- Difficulty
- medium
Related questions
Q1. Diesel engines featuring open combustion chambers operate by____________________?
Show answer Hide answer
Answer: A. the shape and layout of the piston crown, the inlet port, and the valve produce the turbulent effect on fuel mixture
Open combustion chamber diesel engines rely on direct fuel injection into a single unified cylinder volume. Engine designers shape the piston crown and intake ports to generate intense air swirl and turbulence. This high...
Q2. Preventing carbon deposits on fuel injectors requires nozzle tip temperatures to be__________________?
Show answer Hide answer
Answer: C. between 250 – 300°C
Maintaining nozzle tip temperatures within 250-300°C prevents carbon deposits. Higher temperatures cause fuel coking, while lower temperatures encourage deposits. Optimal thermal management ensures clean diesel fuel inje...
Q3. Within a static fluid___________________?
Show answer Hide answer
Answer: D. only normal stresses can exist
In a static fluid at rest, shear stresses cannot exist by definition. Fluid molecules at rest do not slide past one another, eliminating any internal resistance to shear. Therefore, only normal compressive stresses, comm...
Q4. Grey cast iron holds carbon in the form of____________________?
Show answer Hide answer
Answer: C. flakes
Grey cast iron contains carbon exceeding the solubility limit of austenite during solidification cooling. This excess carbon precipitates out of the iron matrix in the structural form of graphite flakes. The exposed grap...
Q5. Locomotive draught is generated using_________________?
Show answer Hide answer
Answer: D. steam jet draught
Steam locomotives generate draught using a steam jet exhaust blast. Exhaust steam discharges into the smokebox to draw combustion gases through tubes. This self-regulating drafting method increases with engine power outp...
Q6. Advancing spark timing in petrol engines results in_______________?
Show answer Hide answer
Answer: A. increase the knocking tendency
Advancing the spark timing causes combustion to occur earlier while the piston is still rising. This premature burning creates extreme peak pressures inside the cylinder chamber. Higher peak pressures dramatically increa...