Mottled cast iron contains carbon in the form of__________________?
Show answer Hide answer
Answer: E. partly in free and partly in combined state
Explanation
Mottled cast iron gets its name from the speckled appearance caused by mixed microstructural phases. During solidification, carbon precipitates partly as free graphite flakes and partly remains combined as iron carbide. This dual nature gives mottled iron properties intermediate between hard white cast iron and soft gray iron. Cast irons are iron-carbon alloys containing more than two percent carbon along with various silicon additions. Graphite represents the free carbon form that provides gray cast iron with excellent machinability and damping capacity. Cementite represents the combined iron carbide phase that imparts extreme hardness and wear resistance to white iron.
Containing carbon solely in free form describes gray cast iron rather than a mottled transitional structure. Having carbon entirely in combined form characterizes hard white cast iron rather than a mixed microstructure. Nodular cast iron features spherical graphite nodules rather than the mixed free and combined carbon state.
- Subject
- Engineering
- Category
- Mechanical Engineering
- Topic
- —
- Difficulty
- medium
Related questions
Q1. Under compression, a brittle material prism fails by________________?
Show answer Hide answer
Answer: A. by forming a bulge (l>) by shearing along oblique plane
Brittle materials under compression fail by shearing along an oblique plane. Unlike ductile metals, brittle prisms shatter or crack along diagonal slip lines. Compressive stress exceeds the shear strength along specific...
Q2. Multi-cylinder petrol engine ignition timing is adjusted by_________________?
Show answer Hide answer
Answer: D. rotating the distributor
Rotating the distributor housing alters the angular timing of the spark across multi-cylinder engines. This mechanical adjustment advances or retards when the spark plug fires relative to piston position. Physical rotati...
Q3. Forced-recirculation boilers operate by__________________?
Show answer Hide answer
Answer: C. feed pump is employed to supplement natural circulation in water wall type furnace
Forced-recirculation boilers use an auxiliary pump to actively assist natural water circulation paths. The circulation pump ensures adequate coolant flow through furnace water walls during heavy firing. Mechanical assist...
Q4. Preventing carbon deposits on fuel injectors requires nozzle tip temperatures to be__________________?
Show answer Hide answer
Answer: C. between 250 – 300°C
Maintaining nozzle tip temperatures within 250-300°C prevents carbon deposits. Higher temperatures cause fuel coking, while lower temperatures encourage deposits. Optimal thermal management ensures clean diesel fuel inje...
Q5. Within a static fluid___________________?
Show answer Hide answer
Answer: D. only normal stresses can exist
In a static fluid at rest, shear stresses cannot exist by definition. Fluid molecules at rest do not slide past one another, eliminating any internal resistance to shear. Therefore, only normal compressive stresses, comm...
Q6. Nodular iron contains graphite structured as_____________________?
Show answer Hide answer
Answer: D. spheroids
Nodular cast iron contains graphite arranged in distinct spheroidal or nodular shapes. Special treatment of the molten metal transforms sharp graphite flakes into rounded spheres. Spheroidal graphite stops stress concent...