Cast iron is generally characterized by_________________?
Show answer Hide answer
Answer: B. its elastic limit close to the ultimate breaking strength
Explanation
Cast iron exhibits brittle material behavior with very limited plastic deformation capacity. Its elastic limit sits exceptionally close to its ultimate breaking strength under load. Once stress surpasses the elastic limit, cast iron fractures without significant yielding. Cast iron contains high carbon and silicon concentrations, leading to graphite flake formation. Brittle materials fracture suddenly under tension without warning plastic elongation. Mechanical testing graphs show a nearly straight elastic line terminating abruptly at fracture.
Machine tool bases and engine blocks use cast iron for its rigidity and vibration damping. Engineers avoid using cast iron in applications subject to high tensile shock loads. Understanding brittle fracture limits prevents catastrophic structural failures in machinery. Option A is incorrect because cast iron has relatively low tensile strength compared to steel. Option C is incorrect because cast iron is brittle and lacks significant ductility. Option D is incorrect because options A and C do not describe cast iron properties.
- Subject
- Engineering
- Category
- Mechanical Engineering
- Topic
- —
- Difficulty
- medium
Related questions
Q1. Capillary fluid phenomena are driven by_________________?
Show answer Hide answer
Answer: D. all of the above
Capillary action is driven by surface tension forces acting along the liquid-gas interface boundary. Cohesion forces between liquid molecules pull the fluid together and maintain droplet integrity. Adhesion forces betwee...
Q2. The presence of carbon within an iron matrix exemplifies__________________?
Show answer Hide answer
Answer: B. interstitial solid solution
Iron possesses a crystal lattice structure with empty interstitial spaces located between its larger metallic atoms. Carbon atoms are sufficiently small to slip directly into these interstitial voids without disrupting t...
Q3. Brass alloy is made up of___________________?
Show answer Hide answer
Answer: A. 70% copper and 30% zinc
Brass is a versatile metal alloy formed by combining copper with zinc alloying elements. Standard yellow brass compositions consist of approximately seventy percent copper by weight. The remaining thirty percent of the a...
Q4. Carburetion processes are executed to________________?
Show answer Hide answer
Answer: C. break up and mix the petrol with air
Carburetion is the mechanical process of atomizing liquid petrol into microscopic droplets. Atomized petrol is thoroughly mixed with incoming air to create a combustible air-fuel charge. This homogeneous mixture is then...
Q5. An unsealed water container undergoes upward acceleration along an inclined plane. The free liquid surface will tilt in what manner__________________?
Show answer Hide answer
Answer: C. make an angle in opposite direction to inclination of inclined plane
An unsealed container accelerating upward along an inclined plane experiences combined gravitational and inertial forces. The resultant acceleration vector acts at an angle relative to the vertical plane of the container...
Q6. The specific calorific energy of mineral coal falls within the range of_______________________?
Show answer Hide answer
Answer: C. 2000-4000 kcal/kg
The specific calorific value of mineral coal typically falls within the range of 5000 to 8000 kcal/kg, making option C incorrect.